Chemical Interactions Between Cement And E-Glass Fibres With A Cao-Ba0-Si02-Tio2 Coating

E-glass fibres were coated with a 15CaO-15BaO-20SiO2-50TiO2 thin film by the sol-gel method. Mechanical and chemical tests were performed on coated and uncoated fibres in cement and cement extract solutions to investigate the interactions between cement and gel-glass film The results show that the resistance of E-glass fibres to the alkali cement medium is enhanced by the 15 CaO-15BaO-20SiO2-50TiO2 coating. The significant roles of TiL2, CaO, and BaO in the protection fibres from the alkaline attack of cement are described. Some evidence is presented that the alkali corrosion of the coated fibres results in the formation of a thick and compact Ti film that suppresses further corrosion reaction.

Author
L Wen Et Al
Origin
University Missouri-Rolla, Usa
Journal Title
J Am Ceram Soc 88 12 2005 3507-3508
Sector
Glass Fibre
Class
GF 490

Request article (free for British Glass members)

Chemical Interactions Between Cement And E-Glass Fibres With A Cao-Ba0-Si02-Tio2 Coating
J Am Ceram Soc 88 12 2005 3507-3508
GF 490
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.