Chemical Imaging Of Glass Surfaces By Mass Spectrometry

This article reviews the basic elements of TOF-SIMS instrumentation and illustrates the power of this approach by examining the mass spectra of coated and uncoated glass fibres.

Author
C G Pantano Et Al
Origin
Pennsylvania State University
Journal Title
The Glass Researcher 9 1 1999 22-23
Sector
Special Glass
Class
S 1781