The Chemical Durability Of Silicate Glass: Conclusion

Following a discussion of the resistance properties of optical and fiber glass, the author sums up his review with a description of general testing procedures and annoted bibliography on chemical resistance in glass.

Author
F R Bacon
Origin
Owens-Illinois
Journal Title
Glass Industry October 1968 554-559
Sector
Primary Papers
Class
PP 1191