Chemical Degradation And Chromophores Of 18Th Century Window Glasses

Three sets of glass samples from 18th century leaded windows from the Girona Cathedral, Reus Priory Church and the Vitoria Cathedral (Spain) have been studied. Chemical analyses and archaeometry of these glasses are of special interest due to both the scarcity of 18th century stained glass window production and to the particular orange colour of several glass pieces. Chemical degradation of glasses has been deduced from their composition and conservation state, directly observed using optical and electron microscopy. The chemical species responsible for colouring (chromophores) and other chromatic parameters have been investigated from optical spectroscopic data. The results indicated that glasses from Girona Cathedral are potash-lime-silica glasses, whereas those of the Reus Priory Chruch and Vitoria Cathedral are soda-lime-silica glasses. The durability of the glasses studied is directly related to their respective chemical composition: potash glasses from Girona show advanced chemical degradation, compared with the other sets of glasses analysed.

Author
T Palomar Et Al
Origin
Inst History, Cchs-Csic, Spain
Journal Title
Glass Technology (Eur J Glass Sci) 52 5 October 2011 154-153
Sector
Special Glass
Class
S 3744

Request article (free for British Glass members)

Chemical Degradation And Chromophores Of 18Th Century Window Glasses
Glass Technology (Eur J Glass Sci) 52 5 October 2011 154-153
S 3744
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.