Chemical Composition Of Medieval Glass From Excavations In West Germany

Investigations of excavated glass fragments from many towns, including the Roman-Frankish cemetery at Kredfeld-Gelle, have been examined and conclusions regarding technical procedures used at the time analysed.

Author
K Hans Wedepohl
Origin
Geochemisches Inst Der Universitat Gottingen, Germany
Journal Title
Glastech Ber Glass Sci Technol 70 8 1997 246-255
Sector
Special Glass
Class
S 1220