Chemical Composition Analysis Of Alkali Borate And Alkali Germanate Glasses

Borate and germanate anions in aqueous solution combine with two molecules of mannitol to form a borate mannitol complex or a germanate mannitol complex if sufficient mannitol is present. The formation constants of these two complexes are in close agreement which indicates a striking chemical similarity between these two complexes. Both complexes are moderately strong acids so that the compositions of alkali borate and alkali germanate glasses can be determined by the same potentiometric titration method.

Author
M Kodama Et Al
Origin
Sojo University, Japan
Journal Title
Glass Technology 44 2 2003 50-58
Sector
Special Glass
Class
S 2712

Request article (free for British Glass members)

Chemical Composition Analysis Of Alkali Borate And Alkali Germanate Glasses
Glass Technology 44 2 2003 50-58
S 2712
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.