Chemical Analysis Of Some Elements In Oxidation-Reduction Equilibria In Silicate Glasses

Techniques and procedures useful for quantitative measurements of the oxidation reduction equilibria of 13 elements are described: Fe,S,Cu,Sb,As,V,Mn,Se,Cr,Ce,U,Sn and Ti. These techniques are procedures are adaptable to concentrations as low as a few ppm in the sample. Analyses of combinations of some of these elements and of copper ruby, manganese brown, ultraviolet absorbing green, iron sulphur amber and selenium pink commercial glasses are given.

Author
Wp Close & Jf Tillman
Origin
Unknown
Journal Title
Glass Technology 10 5 1969 134-146
Sector
Primary Papers
Class
PP 1330

Request article (free for British Glass members)

Chemical Analysis Of Some Elements In Oxidation-Reduction Equilibria In Silicate Glasses
Glass Technology 10 5 1969 134-146
PP 1330
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.