Chemical Analysis Of Ancient Glasses By Energy Dispersion Spectrometry On An Electron Microscope (S.D.E.) And By Microprobe. (In French)

Scanning, electron microscopy and microprobe techniques have been used for the analysis of more than a hundred samples of ancient glasses and the merits of this type of approach are discussed.