Cheaper Coloured Glass Bottles Are On The Way

Bottles from Lax and Shaw coloured by the Vapocure coating process should come on the market in about three months. Blue bottles are currently being supplied to G J Greenall of Warrington at two-thirds the cost of those based on using blue feeder glass, according to the article.