Characteristics Of The Raw Materials For Melting Different Types Of Glass (Spanish)

The factors affecting the selection of raw materials, specifications for sand and limestone, the use of cullet, and minerals such as feldspar, clay and rocks are discussed with reference to the literature.

Author
J M Fernandez Navarro
Origin
Instituto De Ceramica Y Vidro
Journal Title
Bol Soc Esp Ceram Vidr 1989 28 6 449-459
Sector
General
Class
G 383