Characterisation By Optical Methods Of Coatings On Architectural Glazings (Italian)

It is shown that optical characterisation of the coatings on flat glass, including thickness determination, refractive index and absorption coefficient, facilitates prediction of performance in terms of the energy balance of glazed buildings.