Changing The Rules On Forehearth Dimensions

Optimisation of the cooling configurations in the PSR System 500 forehearth has dramatically increased the level of control available to its operators. The improved performance of these conditioning systems has also made some of the traditional assumptions about the necessary size of forehearths inappropriate.

Author
J Mcminn
Origin
Parkinson Spencer Refractories
Journal Title
Glass 74 3 1997 111-112
Sector
Container glass
Class
C 1036

Request article (free for British Glass members)

Changing The Rules On Forehearth Dimensions
Glass 74 3 1997 111-112
C 1036