Change In Refractive Index Of A Borosilicate Glass Fibre Annealed Below The Glass Transformation Temperature

Glass fibres pulled from multihole bushings can have a slight difference in thermal history that causes a distribution in the refractive index that can be narrowed by annealing the fibres.