Challenging Conditions For Cis Container Sector

The Commonwealth of Independent States is a regional organisation, whose participating countries are former Soviet Republics, created during the break-up of the Soviet Union. In this article the author discusses the glass container industry in Ukraine, Belarus and Uzbekistan. Sadly, at the time of writing, political unrest in parts of the Ukraine was making headlines of a different kind throughout the world.

Author
D Singh
Origin
Unknown
Journal Title
Glass Worldwide May-June 2014 106, 108, 110