Cesium Speciation In Nuclear Waste Glasses

Cesiums ion specification in sodium cesium borosilicate and sodium aluminophosphate glasses potentially suitable for immobilization of Cs-containing radioactive wastes or ionizing radiation sources was studied using x-ray absorption spectroscopy (XAS).

Author
S V Stefanovsky & J J Purans
Origin
Sia Radon, Russia, & Inst Solid State Physics, Latvia
Journal Title
Phys Chem Glasses 53 5 2012 186-190
Sector
Special Glass
Class
S 3967

Request article (free for British Glass members)

Cesium Speciation In Nuclear Waste Glasses
Phys Chem Glasses 53 5 2012 186-190
S 3967