Cerberite Break-Through Eliminates Finish Defects

Johnson Radley's Cerberite development programme has led to a new application for the hot end handling material. The new Cerberite 50 top plate eliminates a long-standing cause of finish defects in glass containers.

Author
T Legood
Origin
Johnson Radley, Uk
Journal Title
Int Glass Journal July-Sept 93 1997 40-41