Ceramic Welding Is A Value Added Means Of Extending Gas/Oxy Furnace Life

Today's glass manufacturers are operating melting furnaces that are becoming more environmentally friendly. One method of achieving this goal, which is becoming increasingly acceptable in application, has been the introduction of the gas/oxy combustion systems. Although some regenerative furnaces have used gas/oxy burners to boost production or reduce exhaust gas volume, the preferred, and typically most cost-effective furnace design for utilising this type of combustion system, is the direct-fired melter.

Author
C M Zvosec
Origin
Fostel Inc, Usa
Journal Title
International Glass Review 1 1998 35-36, 38
Sector
General
Class
G 1841

Request article (free for British Glass members)

Ceramic Welding Is A Value Added Means Of Extending Gas/Oxy Furnace Life
International Glass Review 1 1998 35-36, 38
G 1841
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.