Ceramic Tile Scratch Resistance: Determination Of Scratch Parameters

A test method has been fine-tuned for quanitfying the scratch resistance of ceramic tile surfaces by determining two parameters: Qr (load required to produce a scratch) and Qd (load required to produce chipping). The scratches were made by a scratch tester fitted with a diamond tip. To suppress the influence of surface appearance (colour and gloss) on test results, a topographic map of the scratched area, made with a roughness meter, was used to observe the scratches. This method was applied to the surface of several glazes and the relation of parameters Qr and Qd to glaze mechanical properties (wear resistance and toughness) was studied.

Author
A Escardino Et Al
Origin
Universitat Jaume, Spain
Journal Title
Cfi/Ber 79 9 2002 E24, E26
Sector
Glass Ceramics
Class
GC 464

Request article (free for British Glass members)

Ceramic Tile Scratch Resistance: Determination Of Scratch Parameters
Cfi/Ber 79 9 2002 E24, E26
GC 464
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.