The Ceramic Revolution

After more than two years of research, materials scientists at AEA Industrial Technology, in collaboration with Portmeirion Potteries, H&R Johnson Tiles and Diamond Refractories (all UK), have discovered new routes and uses for the sol-gel process, one of which is for the advancement of the decoration of tableware.