Ceramic Powder Synthesis By Spray Pyrolysis

A variety of spray pyrolysis (SP) techniques have been developed to directly produce ceramic powders from solutions. This paper reviews the current status of these processes in terms of the process parameters that enable the formation of particles with controlled morphology and composition. A model incorporating solute diffusion in the droplet and solvent evaporation from the droplet surface is presented to establish the critical parameters leading to solid particle formation.

Author
G L Messing Et Al
Origin
Pennsylvania State University, Usa
Journal Title
J Am Ceram Soc 76 11 1993 2707-2726
Sector
Glass Ceramics
Class
GC 147

Request article (free for British Glass members)

Ceramic Powder Synthesis By Spray Pyrolysis
J Am Ceram Soc 76 11 1993 2707-2726
GC 147
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.