Ceramic Kilns With Improved Environmental Protection

Modern materials have made a decisive contribution to energy saving during firing processes. This paper surveys the different types of kiln linings currently available. The contaminants - in particular fluorine and hydrocarbons - can be neutralized with dry sorption plants and purpose-built post-combustion systems. These systems are also presented.

Author
R Sladek
Origin
Nuremberg
Journal Title
Cfi/Ber Dkg 71 9 1994 531-534
Sector
Glass Ceramics
Class
GC 168

Request article (free for British Glass members)

Ceramic Kilns With Improved Environmental Protection
Cfi/Ber Dkg 71 9 1994 531-534
GC 168