A two-step processing route for ceramic foams has been developed at VITO, Materials Technology, Belgium. The ceramic foams have sufficient strength and controlled microstructures. The process involves preparing structures that are built up by ceramic hollow spheres with a fixed diameter and then connected together. The ceramic hollow spheres are produced using a sacrificial coating technique. These spheres are packed into a mold, joined together using a second slurry coating, calcined and finally, sintered. Lightweight materials with densities as low as 10% of theoretical density were obtained. For more information please contact J Luyten, email: [email protected]

Author
Un-named
Origin
Unknown
Journal Title
American Ceramic Soc Bulletin 83 May/04 4
Sector
Special Glass
Class
S 2796

Request article (free for British Glass members)

Ceramic Foam Processing
American Ceramic Soc Bulletin 83 May/04 4
S 2796
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.