Ceramic Engineering Today And Tomorrow: Impact On Energy

Ceramic materials have been involved in the generation, transmission and consumption of electrical energy throughout its history, and they will continue to be important in the future.

Author
M L Korwin
Origin
Nys College Of Ceramics, Usa
Journal Title
Am Ceram Soc Bull 76 12 1997 47-50
Sector
Glass Ceramics
Class
GC 298

Request article (free for British Glass members)

Ceramic Engineering Today And Tomorrow: Impact On Energy
Am Ceram Soc Bull 76 12 1997 47-50
GC 298