Ce Marking

From March 1st 2007, all glass products from the second group (insulating glass, laminated glass, and tempered glass submitted to HST) intended for use in the building sector will have to carry a CE mark. GlassOnWeb.com dedicates, for the second consecutive week, the focus article to the mandatory CE marking, as it is a far serious and important issue for the industry. What is the CE mark and what changes will it bring? This article answers most of the questions relating to glass issues.