Cation And Network Structure In Binary Potassium Borate Glasses

XFAS studies of network modifying cations in alkali borate glasses have made an important contribution to the understanding of the structure of glass. Using a laboratory XAFS facility, the local structure in K2O-B2O3 glasses has been determined in order to elucidate the environment of network modifying K+ ions. The average coordination umber, Nk-o, of oxygen around K+ cations and the mean distance, Rk-o, for K-O correlations are found to be approximately 6 and 2.83-2.86 A, respectively. The XAFS results are in good agreement with X-ray diffraction and MD simulation results.

Author
N Umesaki Et Al
Origin
Osaka National Research Inst, Japan
Journal Title
Proc 2Nd Int Conference Borate Glasses, Crystals & Melts 1996 99-106
Sector
Special Glass
Class
S 3648

Request article (free for British Glass members)

Cation And Network Structure In Binary Potassium Borate Glasses
Proc 2Nd Int Conference Borate Glasses, Crystals & Melts 1996 99-106
S 3648
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.