Casting Shapes At Zedmark

Casting ceramic-bonded refractories at the Slippery Rock, Pa plant of the Zedmark Division of Quigley is described. Products for the glass industry include orifice rings, plungers, rotor segments, stirrers, channels and superstructure parts, spouts, spout burners and covers.