The Cast Glass-Ceramic Restoration

The use of Dicor glass-ceramic material for fixed prosthodontic complete crowns is described.

Author
K A Malament, D G Grossman
Origin
Corning Glass Works
Journal Title
J Prosthetic Dentistry 1987 57 6 674-683
Sector
Glass Ceramics
Class
GC 17

Request article (free for British Glass members)

The Cast Glass-Ceramic Restoration
J Prosthetic Dentistry 1987 57 6 674-683
GC 17