[Case Study] Msc & Sgcc: Wiegand Glas Experiences Its First Atlas System For Non-Contact Check Detection

Back in June, Wiegand Glas installed its first ATLAS system dedicated to the non-contact detection of checks in the ring, the neck, the shoulder and the bottom areas of glass containers. The ATLAS system is operational at Steinbach am Wald glass plant in Germany. MSC & SGCC supplier of control quality solutions, had the opportunity to meet with Alexander Treuner - cold-end Quality Control Manager and Daniel Rosse - ATLAS Project Leader, to discuss their experience of the ATLAS solution.

Author
Un-named
Origin
Unknown
Journal Title
Gmpa 5/10 58-61
Sector
Container glass
Class
C 4260

Request article (free for British Glass members)

[Case Study] Msc & Sgcc: Wiegand Glas Experiences Its First Atlas System For Non-Contact Check Detection
Gmpa 5/10 58-61
C 4260
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.