A Case For Automated Thickness Measurement

Studies have shown that material distribution is the one attribute that most impacts bottle performance. As we move along the path of increased lightweighting and complex glass container designs, the author of this paper explains how the proper distribution of material is becoming increasingly important.

Author
D Dineff
Origin
Agr Usa
Journal Title
Glass International April 2013 71-72
Sector
Container glass
Class
C 4877