Camera Control Systems Improve Efficiency In Ocmi Machines

Camera control systems developed by Italian-based OCMI for tube forming machines reduce glass waste, keep the sizes of glass containers inside tighter tolerances, and avoid troubles during after-forming operations, according to this article. Ref: GMPA 6/2014 27-29