Calculations Of The Effective Magnitudes Of The Rates Of Longitudinal And Lateral Flow Of Glass In Tank Furnaces

The movement of glass with single-cycle and two-cycle convection in glass tank furnace is discussed and a method is proposed for calculating the flow of white glass in narrow channels with reference to the effect of convection.

Author
K.A. Pchelyakov And A.A. Sokolov
Origin
Unknown
Journal Title
Glass And Ceramics 1968 25 (11-12) 649-653