The Calculation Of Phase Separation Kinetics In Metastable Systems For Two Models Of Particle Nucleation

The kinetics of the nucleation-growth type phase separation for two models with diffusion-limited growth of spherical particles has been calculated. Some results of experimental study of phase separation in glasses are mentioned which are in agreement with results of presented theoretical analysis.