Calcluations On Fluoride-Opacified Glasses And The Loss Of Fluorine During Glassmelting

The methods of Jochmann and Beyersdorfer (1949) for calculating the batch mixture from analysis of the glass are considered unsatisfactory and full details of a better method are given.