Calcium Phosphate Bioceramics With Various Porosities And Dissolution Rates

Porous bioceramics, such as hydroxyapatite (HA), tricalcium phosphate (TCP), and biphasic HA/TCP, were fabricated using the polyurethane sponge technique. The porosity of the ceramics was controlled by a multiple coating of the porous body. When a porous body was produced by a single coating, the porosity was ~90%, and the pores were completely interconnected. When the sintered body was coated five times after the porous network had been made, the porosity decreased to 65%. As the porosity decreased, the strength increased exponentially. The TCP exhibited the highest dissolution rate in a Ringer's solution, and the HA had the lowest rate. The biphasic HA/TCP showed an intermediate dissolution rate.

Author
S Kwon Et Al
Origin
Seoul Nat Univeristy, Korea
Journal Title
Ja M Ceram Soc 85 12 2002 3129-3131
Sector
Glass Ceramics
Class
GC 501

Request article (free for British Glass members)

Calcium Phosphate Bioceramics With Various Porosities And Dissolution Rates
Ja M Ceram Soc 85 12 2002 3129-3131
GC 501
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 16 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.