Calcium Hydroxide Saturation Factors In The Pore Solution Of Hydrated Portland Cement Fly Ash Pastes

The portlandite saturation factors in the pore solution of hydrated portland cement paste and changes related to the addition of two types of fly ash have been studied. Small additions (15wt%) of fly ash increase portlandite supersaturation at early ages, whereas larger additions reduce it, relative to the plain cement. At later ages, portlandite undersaturation is observed despite the continued presence of free portlandite in the paste as observed by SEM.

Author
S Goni Et Al
Origin
Inst Construction Science, Madrid, Spain
Journal Title
J Am Ceram Soc 79 4 1996 1041-1046
Sector
Special Glass
Class
S 998

Request article (free for British Glass members)

Calcium Hydroxide Saturation Factors In The Pore Solution Of Hydrated Portland Cement Fly Ash Pastes
J Am Ceram Soc 79 4 1996 1041-1046
S 998
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.