Burner Design And Operation In The Melting And Conditioning Of Glass

The factors that need to be considered in the design of a glass furnace are discussed with particular reference to the various fuel injection and burner systems currently available.

Author
R S Pont
Origin
Laidlaw Drew Limited
Journal Title
Glass Production Technology International 1990 73-77
Sector
General
Class
G 419