Bulk Glass Formation Of 12Mm Rod In La-Cu-Ni-Al Alloys

Microstructures of La-Cu-Ni-Al alloys of rod samples with 12mm diameter prepared by copper mould casting along La86-x compositional line were studied by scanning electronic microscope (SEM) observation, and X-ray diffraction (XRD). Glassy rod with diameter of 12mm can be formed by copper mould casting.

Author
Y Zhang Et Al
Origin
National University Singapore
Journal Title
Materials Science & Engineering A375-377 2004 436-439
Sector
Special Glass
Class
S 3115

Request article (free for British Glass members)

Bulk Glass Formation Of 12Mm Rod In La-Cu-Ni-Al Alloys
Materials Science & Engineering A375-377 2004 436-439
S 3115