A Bright Future Ahead For Heat Release Decals

In this paper the author looks at the use of heat release decals and explains how the technology has developed to provide a high quality glass surface decoration.

Author
P Hesp
Origin
Service (Engineers) Plc, Uk
Journal Title
Glass International, November 1998 33-34
Sector
Container glass
Class
C 1247