Breaking The Limit Of Oxide Glass Microductility

This article looks at how university researchers have created a microductile oxide glass with crack resistance more than ten times higher than previous glasses.

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 98 7 September 2019 11
Sector
Special Glass
Class
S 4534

Request article (free for British Glass members)

Breaking The Limit Of Oxide Glass Microductility
Am Ceram Soc Bull 98 7 September 2019 11
S 4534