[Brazil] Guardian Begins Production At Second Brazilian Float Plant

Production is underway at Guardian Industries' newest float site in Brazil. It is reported the plant, based in Tatui, Sao Paolo, will have an output of 800/tpd and will create 300 jobs. The facility was constructed in response to the success of Guardian's other Brazilian site, located in Porto Real, which has been in operation 10 years. This plant has also extended its operations with the addition of a state-of-the-art coating machine. According to reports, Guardian's investments in the country total over US$ 180M.

Author
Un-named
Origin
Unknown
Journal Title
Glass International June 2009 3
Sector
Flat glass
Class
F 2737

Request article (free for British Glass members)

[Brazil] Guardian Begins Production At Second Brazilian Float Plant
Glass International June 2009 3
F 2737
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.