Zippe Industrieanlagen announced it has received an order for a batch plant with a maximum capacity of 400 t/d from Brazilian container glass manufacturer Vidroporto. The batch plant is part of an order to install a fully automatic cullet return system for the new furnace F3 in Porto Ferreira, Brazil. Apart from the equipment and the complete control system, the order also includes the steelwork, and is scheduled for commissioning in the second quarter of 2014.