Branding Opportunities Cast The Mould For Glass

The upswing in demand for glass containers over the last three years is discussed briefly with special reference to the use of colour and shape to create brand personality.

Author
C Hall
Origin
Unknown
Journal Title
Packaging News January 1990 16-18