Borosilicate As An Important Component In The Glass World

By glass, we normally mean an "oxide glass" and for most of our day-to-day applications, we mean silicate glasses - mainly a variety of soda-lime-silica glasses for different usages, such as containers for home and industrial applications, float glass for building construction, and other applications. However, there are various other types of non-silicate glasses (borates, borophosphates, alumino phosphates, boro-aluminophosphates etc) for many types of applications requiring special properties. Among all these glasses encompassing a wider composition base, the borosilicate glasses stand apart in terms of an impressive list of applications at home as well as in the scientific and industrial fields. This article provides a description of borosilicate glass with a flavour of their various usages.

Author
Prof A K Bandyopadhyay
Origin
West Bengal Unviersity Technology, Kolkata
Journal Title
Kanch 3 4 2016 41-45
Sector
General
Class
G 4488

Request article (free for British Glass members)

Borosilicate As An Important Component In The Glass World
Kanch 3 4 2016 41-45
G 4488
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.