Borosilicate Glass Defects And Selected Refractory Materials

The focus of this work is exclusively on the borosilicate family of glasses which can produce some unique defects. Only those defects related to the melting and delivery of the glass will be discussed. It is hoped that the makers of borosilicate products will benefit from a reference with this focused perspective.