Boron Phosphate Glass-Ceramics

The extent of glass and glass-ceramic formation in the B2O3-P2O5-SiO2 system is described where homogeneous nucleation and growth of submicroscopic BPO4 crystallites are induced during heating of the quenched glasses.

Author
J F Macdowell
Origin
Corning Glass Works
Journal Title
Proc Xv Int Cong Glass, Leningrad 1989 3A 90-95