Bormioli Rocco - New Glass Range Developed

Bormioli Rocco's pharmaceutical division has developed a new range of glass containers named "Bormio-Lyo." The company has implemented a new production technology that achieves a 30% reduction in weight, making its glass vials very similar to tubular vials in weight and design.