Borate Structures By Vibrational Spectroscopy

This paper deals with some recent contributions of infrared and Raman spectroscopies to the structural description of borate systems. It demonstrates how the vibrational spectra can assist the decoding of local and intermediate range structure of crystals and glasses.

Author
G D Chryssikos & E I Kamitsos
Origin
Nat Hellenic Research Foundation, Greece
Journal Title
Proc 2Nd Int Conference Borate Glasses, Crystals & Melts 1996 128-139