Bone Formation At A Ceramic Implant Interface

A nonporous ceramic implant in rat femora was evaluated as to its ability to bond to bone. A number of morphologic techniques were utilised to examine the interfacial relationship of the implant to new bone. Transmission electron microscopy and fluorescence microscopy after tetracycline labelling were the most successful techniques. An intimate relationship between mineralised bone and the ceramic was demonstrated by transmission electron microscopy. The appearance of tetracycline labelling at the ceramic interface indicates that the implant may have capacity to enhance bone formation.

Author
C A Beckham Et Al
Origin
University Florida, Usa
Journal Title
Calc Tiss Res 8 1971 165-171
Sector
Glass Ceramics
Class
GC 784

Request article (free for British Glass members)

Bone Formation At A Ceramic Implant Interface
Calc Tiss Res 8 1971 165-171
GC 784
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.