Bonding Mechanisms At The Interface Of Ceramic Prosthetic Materials

The development of a bone-bonding calcia-phosposilicate glass ceramic is discussed. A theoretical model to explain the interfacial bonding is based upon in-vitro studies of glass-ceramic solubility in interfacial hydroxyapatite crystallisation mechanisms, compared with in-vivo rate femur implant histology and ultrastructure results.

Author
L L Hench Et Al
Origin
University Of Florida, Usa
Journal Title
J Biomed Mat Res Symp 2 (Part 1) 1971 117-141
Sector
Glass Ceramics
Class
GC 780

Request article (free for British Glass members)

Bonding Mechanisms At The Interface Of Ceramic Prosthetic Materials
J Biomed Mat Res Symp 2 (Part 1) 1971 117-141
GC 780