Blue Upconversion Emission In Germanate Glass Co-Doped With Yb3+/Tm3+ Ions

In this paper, the upconversion luminescence of 70GeO2-30[Ga2O3-BaO-Na2O] glass co-doped with Yb3+/Tm3+ ions was investigated.

Author
D Dorosz Et Al
Origin
Bialystok University Of Technology, Poland
Journal Title
Int J Appl Glass Sci 5 4 2014 393-400
Sector
Special Glass
Class
S 4160